The best roll-tooth material depends on abrasion and impact duty. Compare manganese steel, alloy cast steel and specialised wear systems before choosing a replacement tooth or segment.
The material that wears least in one application may crack or fail to work harden in another. Assess feed size, hardness, abrasiveness, impact loading and the tooth geometry before specifying a material.
Use the machine drawing and the previous failure pattern to determine whether the main issue is abrasive loss, impact fracture, mounting wear or a combination of mechanisms.
Grades such as ZGMn13 and other manganese-alloy steels are used where suitable loading can promote surface work hardening while the interior retains toughness.
The initial and in-service hardness depend on the grade, heat treatment and operating history. A fixed hardness increase or a guaranteed absence of fracture should not be assumed for every tooth.
Alloy cast steels offer another route to a balance of strength, wear resistance and toughness. Composition and heat treatment should be selected for the tooth section, loads and intended service.
The fact that a casting contains chromium, molybdenum or another alloying element does not by itself establish its performance. Agree the actual material grade and the relevant acceptance requirements.
Tungsten-carbide-containing hardfacing may be considered for some abrasive duties, subject to compatibility with the base material, the component design and the repair or manufacturing procedure.
Ceramic rolls and ceramic-containing systems serve selected applications, including some specialised processing equipment. They should not be presented as universal substitutes for crusher roll teeth that carry substantial impact loads.
Casting integrity, section transitions, heat treatment and mounting dimensions all affect reliability. An integral casting or a graded treatment still requires appropriate process control and inspection; the process name alone does not guarantee against tooth loss or fracture.
For a comparison, record operating hours or processed tonnage together with feed conditions and wear measurements. Send Red Apple Casting the tooth or segment drawing, machine model, specified material and photographs of any damage so that the replacement can be assessed for the actual duty.
For equipment fit, material selection and custom casting enquiries, see our wear parts FAQ or contact Red Apple Casting.
Jaw crusher toggle plate installation must follow the machine-specific procedure. Check the approved part, support surfaces, retention arrangement and post-installation condition before returning to service.
Stop and isolate the machine in accordance with the site procedure and the equipment manufacturer instructions. Secure supported or movable components as required before work starts.
Confirm the toggle plate part number, drawing revision, dimensions and material requirements. Inspect the plate, toggle seats and related parts for wear, cracks or distortion, and clean the relevant contact areas. Prepare the tools and handling equipment specified for the job.
The toggle plate transmits load between the moving-jaw assembly and its supporting arrangement. Its exact position, seating and retention method depend on the crusher design.
Do not assume that every plate is directly fastened to the jaw with a common set of bolts. Follow the machine instructions for fitting, tensioning, fastening and any clearances or lubrication requirements.
Where the toggle is part of a designed overload-protection arrangement, preserve the specified material and strength. An apparently stronger substitute can change the intended behaviour of that arrangement.
Check that the approved contact surfaces are seated correctly and that the specified retention components are fitted. Use the required settings, tightening sequence and torque values for that machine; there is no universal bolt torque or installation gap for all jaw crushers.
Lubricate only the points and surfaces for which the equipment procedure calls for lubrication. If a part does not fit as specified, investigate the drawing, revision and mating components rather than forcing the assembly.
Complete the prescribed mechanical checks before restoring power. Where manual rotation or another functional check is required, use the approved method with the machine made safe for that check.
Return the machine to service using the specified commissioning procedure. Watch for abnormal movement, noise, vibration or loosening and stop for investigation where necessary.
For replacement-part enquiries, provide the machine model, toggle plate and seat drawings, dimensions and the original material specification. Red Apple Casting can review fit and casting requirements against these records.
For equipment fit, material selection and custom casting enquiries, see our wear parts FAQ or contact Red Apple Casting.
Hammer crusher is a commonly used crushing equipment widely used in mining, chemical, metallurgy, building materials, electric power and other industries. Among them, the hammer head is the main wearable part, and the quality of the hammer directly affects the crushing efficiency of the crusher.
At present, most of the domestic hammer crusher hammers are made of high manganese steel. Due to the insufficient wear resistance of high manganese steel, poor wear resistance and short service life, frequent replacement is required.
During the work, the hammer head is also impacted by the material in addition to the impact, so that the long-term repeated use, the working surface of the hammer head will be damaged, and the surface shape will change. Factors affecting the life of the hammer:
1. Structural design and product quality of the hammer
The structural design and geometry of the hammerhead have a great influence on the mechanical properties after heat treatment and the internal metallographic structure. In particular, the hammer head with a large thickness has a more prominent influence. By analyzing the failure modes of the hammerheads of different materials, it is known that the main cause of the hammer head fracture is that there are different degrees of defects inside or on the surface. Due to the presence of defects, most of the hammers are broken at the beginning of use. Therefore, in the production of hammers, reasonable casting and heat treatment processes must be established.
2. Technical parameters of hammer crusher
The technical parameters of the hammer crusher also affect the service life of the hammer, the main one is the power and speed of the rotor. They are not only related to the production capacity of the crusher, but also to the degree of impact hardening of the hammer. The hammerhead has a good degree of impact hardening and its service life is prolonged.
3. The blockiness and hardness of the broken material
The greater the material mass, the higher the toughness requirement, and the higher the material hardness, the higher the hardness requirement of the hammer material. The specific type of crusher should adopt the appropriate feed size, which will extend the service life of the hammer to a certain extent.
4. Adjustment of internal clearance of hammer crusher
The internal clearance of the hammer crusher mainly refers to the gap between the rotor body and the counterattack plate, the purlin and the hammer. The size of these gaps will be related to whether there is accumulation near the purlins and the safety gates. If the stock is present and the hammer cannot press the stack off the stringer, the hammer will be subject to severe friction and wear. Therefore, during use, the gaps between the parts must be adjusted frequently to be within the proper range.
There are many factors influencing the service life of the hammer crusher hammer. The above four points are summarized by the red apple casting according to the production experience of the hammer crusher for many years and the feedback from the customers. For the user's reference of the hammer crusher, For more information, you can consult an expert.
|
Guide:The quality of the wear-resistant hammer is very strict with the casting process. Casting a hammer is a very technical job. The requirements of the manufacturer are not only technical, but also the strength of the enterprise, because it requires that the equipment for casting the hammer must reach a certain level. The casting of the hammer is divided into many parts. The wear resistance of the hammer is affected by various factors, but for the production of the hammer, how to maximize the performance of the wear-resistant material is greatly affected by the manufacturing process. In the production process of the hammerhead, it is first necessary to carry out the process design for the production of the hammerhead, and whether the process design is reasonable and scientific is directly related to the quality of the hammerhead. The process design before production can avoid the defects of the hammerhead and improve the wear resistance. The yield of castings improves the quality of wear-resistant castings. If there are defects in the surface or internal manufacturing of the hammerhead, such as shrinkage cavities, cracks, and through crystals, it will not only reduce the performance of the hammer but also cause the hammer to break. Therefore, reasonable casting and heat treatment processes must be established in the production of hammers. For example, for high-chromium cast iron hammers, vertical pouring and reasonable use of external cold iron should be adopted, and the casting temperature should be strictly controlled. This can make the hammer head have good solidification sequence and feeding conditions in casting, and then obtain dense internal structure. And weaken the phenomenon of coarse grains. The heat treatment process of the hammer determines the realization of its mechanical properties and the distribution of carbides. Since a certain amount of chromium and other alloying elements are contained in the composition of the hammerhead, how to make these alloying elements form a hard spot carbide is fully exerted, which is also a factor to be considered in the heat treatment process. In short, the establishment of a reasonable production process and strict quality inspection methods is a prerequisite for ensuring the performance of the hammer. |
The low price and good economic efficiency are not easy to break. The service life of the high chromium alloy hammer is 4 times that of forged or high manganese steel.